T-FIT Application profile 42 - PVDF UV Resistance

PVDF UV Resistance

ZOTEK® F and a leading competitor were subjected to 200; 400; and 600h accelerated UV exposure using a Xenon tester in rotation mode. Tensile strength was conducted on both exposed and non-exposed samples with ZOTEK F® demonstrating less than 4% loss of strength after 600h compared to a loss of 29% for the competitor.